Classification Temperature
- COM Ceramic Blown fiber 1260° C (2300° F)
- STD Ceramic Blown fiber 1260° C (2300° F)
- HP Ceramic Blown fiber 1260° C (2300° F)
- HA Ceramic Blown fiber 1400° C (2550° F)
- HZ Ceramic Blown fiber 1400° C(2550° F)
Production Technology
- COM Blown Fiber is produced from flint clay by blowing technology.
- STD Blown Fiber is produced from processed flint clay by blowing technology.
- HP and HA Blown Fiber is produced from Alumina/Silica Powder by blowing technology.
- HZ Blown Fiber is produced from Alumina/Silica/zircon Powder by blowing technology.
Working Temperature
- Working Temperature depends on working condition, heating method and environment atmosphere, etc.
Characteristics
- Low thermal conductivity
- Low heat storage
- Excellent chemical stability
- Excellent thermal shock resistance
- No binders, no corrosive agents
- Good sound absorption
Usage
- Material of textile
- Filling material for high-temperature furnace and heating equipment.
Technical index
ITEM |
COM |
STD |
HP |
HA |
HZ |
Specification Temperature° C |
1260 |
1260 |
1260 |
1400 |
1400 |
Working Temperature° C |
<1000 |
1000 |
1100 |
1200 |
1350 |
Color |
White |
White |
White |
White |
White |
Diameter of fiber (µm) |
2-3 |
2-3 |
2-3 |
2-3 |
2-3 |
Chemical composition(%) |
Al2O3 |
44 |
46 |
47-49 |
52-55 |
39-40 |
Al2O3+SiO5 |
96 |
97 |
99 |
99 |
- |
Al2O3+SiO5+ZrO2 |
- |
- |
- |
- |
99 |
ZrO2 |
- |
- |
- |
- |
15-17 |
Fe2O3 |
<1.2 |
<1.0 |
0.2 |
0.2 |
0.2 |
Na2O+K2O |
<=0.5 |
<=0.5 |
0.2 |
0.2 |
0.2 |
|
|
|
|
|
|
All fibers are packed in sack with net weight:20KG/sack